Fact register · PCUDE-S-CIAG-STOP
Alloy semis to alloy wire drawing, Germany (copper)
5 kt
DE · 2024 · Cu copper
± 4 tys. t (standard deviation)
Note: 2024 balance, kt of contained Cu: value reconciled by weighted least squares (WLS); standard deviation after reconciliation 4.0; input data 5.0 ± 4.0 (class C estimate).
How to cite this number
ai-waw.com, AIWAW-2026-PCUDE v1.2, fact PCUDE-S-CIAG-STOP – https://ai-waw.com/przeplyw-metali/przeplyw-miedzi-niemcy